介绍了三种典型高温合金喷射成形坯件的制备工艺,并对其显微组织和力学性能进行了分析和测试.研究表明,喷射成形高温合金坯件整体致密度高,含氧量低,化学成分均匀,组织细小,并具有优异的综合力学性能.
Abstract
The technique of preparing three typical superalloy deposits is introduced.The microstructure and the mechanical properties were analysed and tested.The results indicate that the deposits are integrally dense,and have a low oxygen content,homogeneous chemistry,a refined microstructure,and preferable mechanical properties.
关键词
喷射沉积 /
高温合金 /
显微组织 /
力学性能
{{custom_keyword}} /
Key words
spray-deposition /
superalloy /
microstructure /
mechanical propertie
{{custom_keyword}} /
{{custom_sec.title}}
{{custom_sec.title}}
{{custom_sec.content}}
参考文献
师昌绪,陆达,荣科.中国高温合金四十年.北京:中国科学技术出版社,1996
米国发,田世藩,李庆春等.雾化喷射沉积技术的发展概况及展望.材料科学与工程,1996,14(4):8
中国航空材料手册.北京:中国标准出版社,1989
Liang X,Earthman J C,Lavernia E J.On the Mechanism of Grain Formation during Spray Atomization and Deposition.Acta metall mater,1992,40(11):3003
沈军.雾化沉积过程及其对快凝高温铝合金组织与性能的影响,[博士学位论文]哈尔滨:哈尔滨上业大学.1993
米国发.喷射沉积Ni-Al-Mo系Ni3Al基高温合金及其材料研究,[博士学位论文]哈尔滨:哈尔滨上业大学,1995
{{custom_fnGroup.title_cn}}
脚注
{{custom_fn.content}}